On this page
Several operating conditions change how severely the Peukert effect reduces runtime:
- Chemistry and plate design: Thick-plate flooded lead-acid cells exhibit higher Peukert losses than thin-plate AGM or LiFePO4 cells because electrolyte diffusion inside the plates cannot keep pace with high current.
- Discharge rate relative to C20: Discharges slower than the 20-hour rate (
C/20) can slightly exceed nameplate Ah, while rates aboveC/5(0.2C) rapidly compress available capacity. - Electrolyte temperature: Lowering temperature below 77°F (25°C) increases internal resistance and slows ion diffusion, compounding Peukert loss; at 32°F (0°C), lead-acid high-rate capacity drops sharply, while LiFePO4 packs require charge lockout at <=32°F (0°C) unless self-heated (and BMS minimum charge limits must be checked at <=41°F / 5°C).
- Cutoff voltage: A lower end-of-discharge voltage yields slightly more Ah on paper at the expense of accelerated sulfation in lead-acid cells.
For related DC engineering mechanisms and definitions, see the DC Power Specs glossary.
Peukert Formula and Governing Variables
Peukert's law models runtime t (in hours) at a constant discharge current I (in amps) relative to the battery's rated capacity C (in Ah) at its rated discharge duration H (typically 20 hours for a C20 rating):
t = H * (C / (I * H))^k
Effective capacity C_eff (in Ah) delivered before reaching the specified cutoff voltage at current I is:
C_eff = I * t = C * (C / (I * H))^(k - 1)
When a battery datasheet lists two constant-current discharge ratings (I1, t1) and (I2, t2) measured to the same cutoff voltage and temperature, solve for the Peukert exponent k directly:
k = (log10(t2) - log10(t1)) / (log10(I1) - log10(I2))
| Chemistry | Nominal Bank Voltages | Typical Usable DoD | Illustrative Peukert Exponent (k) |
Primary Runtime Constraint |
|---|---|---|---|---|
| Flooded Lead-Acid | 12.0V / 24.0V / 48.0V | 50% | 1.15–1.30 | Diffusion loss, voltage sag, 50% DoD floor |
| AGM / Gel Lead-Acid | 12.0V / 24.0V / 48.0V | 50% | 1.10–1.20 | Diffusion loss, voltage sag, 50% DoD floor |
| LiFePO4 | 12.8V / 25.6V / 51.2V | 80–90% (default 85%) | 1.02–1.05 | Usable DoD, inverter efficiency, BMS cutoff |
Note: Exponent ranges in the table are illustrative baselines. Always verify the C20, C5, and C1 discharge tables on the specific battery datasheet.
Worked Runtime Example (12V Lead-Acid vs. 12.8V LiFePO4)
Illustrative assumptions:
- Bank nameplate rating: 200Ah at C20 (
C = 200Ah,H = 20h,I_20 = 10A) at 77°F (25°C). - Load: 1,000W continuous AC load on a 120V/60Hz (or 230V/50Hz) inverter at 88% conversion efficiency.
- Average DC bus voltage under load: 12.0V for lead-acid (
I_dc = 1,000W / (12.0V * 0.88) = 94.7A); 12.8V for LiFePO4 (I_dc = 1,000W / (12.8V * 0.88) = 88.8A).
| Battery Type | Exponent (k) |
DC Load (I) |
Full-Cutoff Runtime (t) |
Delivered Ah (C_eff) |
Runtime at Usable DoD |
|---|---|---|---|---|---|
| Flooded Lead-Acid (12.0V) | 1.25 | 94.7A | 1.20 h | 114.0 Ah | ~0.60 h (at 50% DoD) |
| AGM Lead-Acid (12.0V) | 1.15 | 94.7A | 1.51 h | 142.7 Ah | ~0.75 h (at 50% DoD) |
| LiFePO4 (12.8V) | 1.03 | 88.8A | 2.11 h | 187.3 Ah | ~1.79 h (at 85% DoD) |
Without Peukert derating, dividing 200Ah / 94.7A predicts 2.11 hours to 100% DoD for the lead-acid banks. In practice, the flooded bank reaches full cutoff 43% sooner (1.20 hours), and voltage sag under 94.7A pushes constant-power inverter current even higher as the bank discharges.
Steps to Size and Configure Around Peukert Loss
- Collect datasheet discharge points: Obtain the C20 capacity (
C),H = 20h, and at least one higher-rate discharge curve (such as C5 or C1) at the same per-cell cutoff voltage (commonly 1.75V/cell: 10.5V on 12V, 21.0V on 24V, 42.0V on 48V) from the battery nameplate or datasheet. - Calculate or assign
k: Computekfrom two matching-cutoff datasheet points. If only the C20 rating is published, apply a conservative chemistry baseline (1.15for AGM,1.25for flooded lead-acid). - Compute worst-case DC current: Calculate peak continuous DC current at the inverter's low-voltage cutoff (
V_min) and conversion efficiency (I_max = P_ac / (V_min * efficiency)), then plugI_maxinto the Peukert equation to verify that runtime within the usable DoD window (50% lead-acid, 85% default LiFePO4) meets the load requirement. - Program the DC battery monitor: Enter the calculated
kand chemistry charge efficiency factor (typically 85–90% for lead-acid, 99% for LiFePO4) into the shunt monitor so state-of-charge (SoC) tracks usable runtime rather than raw Ah. - Reduce C-rate if runtime falls short: If continuous discharge exceeds
0.3C–0.5Con a lead-acid bank, increase parallel Ah capacity or step the DC bus up from 12V to 24V or 48V nominal (keeping the DC bus strictly <=60V DC) to cut per-cell current.
Sign-Off Criteria
- The Peukert exponent
kprogrammed into the DC shunt matches the value derived from the battery datasheet's same-cutoff discharge curves (or the conservative chemistry baseline if multi-rate data is absent). - Calculated runtime
tat worst-case load current meets required autonomy while staying above the chemistry's usable DoD floor (50% for lead-acid; 80–90% for LiFePO4) and above inverterV_min. - Cold-weather capacity reduction below 77°F (25°C) is factored into winter runtime estimates, and conductor voltage drop between the bank and inverter does not push inverter terminals below
V_minprematurely.
Common Failure Modes
- Premature inverter low-voltage shutdown: Sizing a lead-acid bank by dividing C20 Ah by load amps ignores Peukert loss and internal voltage sag, causing the inverter to trip on
V_minwell before the expected runtime. - Battery monitor SoC drift: Leaving a shunt at a lead-acid default (
k = 1.25) on a LiFePO4 bank causes the display to under-report remaining SoC during heavy loads; settingk = 1.05on a lead-acid bank over-reports remaining SoC until sudden voltage collapse. - Constant-power runaway: AC inverters and regulated DC-DC converters draw constant power (
P = V * I). As Peukert polarization drops terminal voltage, currentIrises, which increasesI^kloss and accelerates cutoff. - Mistaking voltage rebound for usable capacity: Removing a heavy load allows lead-acid open-circuit voltage to recover as electrolyte diffuses back into the plates, tempting operators to restart high-draw equipment that immediately trips
V_minagain. - Computing
kfrom mismatched cutoff voltages: Using a 20-hour rating at 1.75V/cell (10.5V) alongside a 1-hour rating at 1.60V/cell (9.6V) artificially lowerskand overstates high-rate runtime.